Liquid Phase Sintering of Silica
VIPIN KANT SINGH
Pages : 44-48
DOI : 10.1080/0371750X.1981.10822518
Abstract
Si01 has been sintered in the presence of a silicate liquid containing CaO 23 %, AI20 1 15% and Si01 62 %. Silicon dioxide powders of -45 and -75 + 63 micron particle sizes were taken and sintered with 10, 15 and 20% by weight liquid phase. Sintering temperatures were 1250°, 1300°, 1350° and 1400°C and soaking periods were from 1 to 30 minutes. Effects of liquid content of the compact and the sintering temperature were studied for the two particle sizes of Si01• Data were analysed using the empirical equation D = K log t + C and Arrhenius equation. It was found that activation energy of sintering decreased with the increasing amount of liquid phase and -45 micron Si01 sintered with much faster rate than -75 + 63 micron.
Full text : Subscribe to Download Full Text
[Go Back]
 
MAIN PAGE | SITE MAP | PRIVACY POLICY | TERMS & CONDITIONS  | CONTACT US | FEEDBACK
Copyright © 2008-2026 The Indian Ceramic Society. All Rights Reserved

Managed by : htsm